Bullseye glass does not have one firing schedule that suits every project: choose a schedule for the glass thickness, kiln, and intended result, then follow Bullseye’s current kilnforming guidance and adjust cautiously for your setup. A full fuse, tack fuse, slump, and anneal each need different temperature targets or holds, and the annealing and cooling stages matter as much as the peak temperature.
Why There Is No Single Bullseye Schedule
A firing schedule is a sequence of temperature changes and holds, not simply a target temperature. The same Bullseye sheet can need a different schedule depending on whether it is being fused flat, shaped over a mold, or combined with other glass. Thickness, the amount of glass in the kiln, kiln design, and the desired surface all affect how quickly heat reaches the work and how it behaves.
Bullseye’s kilnforming resources provide schedules and guidance for particular project conditions. Use the current schedule or chart that most closely matches your glass and process rather than treating a schedule found online as a universal recipe. If a project combines several conditions, such as thick glass and a mold, the more demanding requirement may govern the firing. When uncertain, check Bullseye’s technical resources or ask the glass supplier for advice on the specific materials.
Schedules may show temperatures in Fahrenheit or Celsius and ramp rates in degrees per hour. Confirm which units your controller uses before programming it. A mistaken unit setting can turn an otherwise sensible schedule into a damaging firing.
What the Parts of a Schedule Mean
Most programmable kiln schedules divide a firing into segments. Each segment specifies how quickly the kiln heats or cools, a target temperature, and sometimes a hold (also called a soak). A hold keeps the kiln near a set temperature for a stated period. The controller then proceeds to the next segment, unless the schedule or kiln operation requires a manual step.
- Heating ramp: The rate at which the kiln rises toward a target. A slower ramp gives heat more time to move through the glass and kiln load.
- Process temperature and hold: The combination that develops the desired degree of fusion or shaping. A higher temperature or longer hold generally changes the result, but the relationship is not a simple one-to-one substitute.
- Rapid cool: A controlled transition from the process temperature toward the annealing range. It is often programmed as fast as the kiln can safely cool, subject to the controller’s limits and the schedule guidance.
- Anneal and annealing cool: A hold and subsequent controlled cooling intended to reduce stress within the glass. The required treatment depends on thickness and construction.
Read the controller’s directions carefully: some controllers ask for a rate, target, and hold for every segment, while others use different labels or conventions. Do not assume that a blank hold, a zero hold, or a rapid-cool entry has the same meaning on every controller.
Choose the Schedule by Process
Start by deciding what the finished piece should look and do. The firing goal determines the process temperature and hold; the glass construction and thickness determine how cautiously it should be heated and annealed.
- Full fuse: The glass pieces are intended to merge into a relatively smooth, unified surface. The exact appearance depends on temperature, hold, glass arrangement, and kiln conditions. A schedule that produces a full fuse in one kiln may produce a different surface in another.
- Tack fuse: The pieces remain visibly raised or retain more of their original shape. Use a schedule designed for tack fusing rather than simply shortening a full-fuse hold without considering the outcome.
- Slumping: The fused or assembled glass softens and bends into a mold. Slumping has its own process target and timing; the mold, glass thickness, and desired depth affect how much heatwork is needed.
- Fire polishing or other surface work: These processes aim to change the surface rather than fully reshape the whole piece. Follow instructions intended for that result and the specific glass construction.
A small test piece can help you judge the visual result before committing a valuable project. Keep the test construction representative: different thicknesses, layers, and decorative materials can change how the glass responds.
Thickness, Construction, and Annealing
Thickness is one of the most important schedule considerations. A piece made from two layers of sheet glass is often treated as a nominal 6 mm construction, but actual thickness can vary, and a project may have thicker areas where pieces overlap. A stack of several layers or a large, solid form needs more careful heat management than a small, thin piece.
Annealing is not just an optional final pause. Glass can retain internal stress after heating and cooling; if it is not cooled appropriately, a piece may crack immediately or fail later. The required annealing treatment increases with the effective thickness and can also be affected by the piece’s shape and uneven thickness. Use the annealing guidance for the thickest relevant section, not merely the thickness of one sheet. For a complex or unusually thick object, consult a specialist schedule rather than extrapolating from a thin project.
Do not open the kiln to speed cooling or check a piece during the annealing stage. Sudden temperature changes can create thermal shock, and opening the lid can interfere with the programmed cool. Let the kiln complete its schedule and cool sufficiently before removing the work, following the kiln and project instructions.
How to Adapt a Schedule to Your Kiln
A schedule is a starting point for a particular combination of glass, kiln, and project, not a guarantee that every kiln will behave identically. Small kilns, large kilns, top-loading and front-loading designs, element condition, thermocouple placement, and the distribution of the load can all influence the result. A heavily loaded kiln may heat differently from the same kiln with one small piece.
- Identify the glass type, total and local thickness, project size, and intended process.
- Find Bullseye guidance that matches those conditions as closely as possible, including the relevant annealing information.
- Check the controller’s units and segment format, then enter each ramp, target, and hold carefully.
- Record the schedule, kiln, load arrangement, and result. Change one variable at a time on later test firings.
When changing a schedule after a result, avoid making several large changes at once. For example, a piece that is less fused than intended could reflect the peak temperature, hold time, kiln calibration, or the way the glass was arranged. A controlled test helps identify the cause. Do not compensate for an unknown firing problem by increasing the peak temperature sharply, especially when the work is thick or includes a mold.
Common Problems and What They Suggest
Firing defects can have more than one cause, so treat these observations as clues rather than a diagnosis. Inspect the piece and the kiln setup, then compare the result with the schedule and material instructions.
- Cracks during or after firing: Possible contributors include thermal shock, insufficient annealing for the effective thickness, uneven thickness, or incompatible glass. Confirm that the materials are intended to be used together and review both the anneal and cooling segments.
- Edges or details look more rounded than planned: The work may have received more heatwork than the intended tack-fuse result. Review the process target and hold, and make a small test before changing a valuable piece’s schedule.
- The piece is not shaped as expected: Check that the schedule matches the slumping or forming goal, and inspect the mold, release, glass placement, and kiln temperature behavior. A longer hold is not automatically the right fix.
- Different areas look different: Uneven glass thickness, placement, heat distribution, or a kiln issue may be involved. Record where the variation occurs and consider whether the load or kiln needs attention.
For repeated unexpected results, verify the controller and thermocouple condition according to the kiln manufacturer’s instructions. A programmed temperature is not necessarily proof that the glass experienced that exact temperature throughout the kiln.
Compatibility and Material Preparation
Bullseye glass is designed to be compatible with other Bullseye glass products that are identified for kilnforming use, but appearance alone does not establish compatibility. Do not assume that another manufacturer’s glass can be combined safely with Bullseye simply because both pieces have a similar color, thickness, or stated coefficient of expansion. Check the product information and compatibility guidance for every material in a fused piece.
Clean glass and careful assembly help make results more predictable. Remove oils, dust, labels, and other contaminants using suitable materials and handling practices. Check that the shelf or mold is prepared with the appropriate kiln wash or release product, and follow that product’s instructions. Contamination, poor mold preparation, or trapped debris can cause defects that changing the firing schedule will not solve.
Safety and Record-Keeping
Use a kiln in accordance with its manufacturer’s operating instructions, with appropriate clearance and ventilation. Kilns and fired glass remain extremely hot after the controller ends a program. Use suitable heat-resistant protective equipment for any task that involves hot materials, and do not handle a piece until it is safe to do so. Keep children, pets, and combustible materials away from the operating kiln.
Maintain a firing log with the date, kiln, controller units, schedule segments, glass and thickness, mold or shelf setup, load placement, and result. A photograph beside the written record can make it easier to compare surface appearance or shape. This is especially useful when a schedule works in one kiln but needs careful adjustment for another.
Frequently Asked Questions
What temperature should I use to full fuse Bullseye glass?
There is no universal full-fuse temperature: the target and hold depend on the desired surface, glass construction, kiln, and controller. Use Bullseye’s current schedule guidance for the project conditions, then test a representative sample if the result is uncertain.
Can I use one schedule for tack fusing and full fusing?
Not reliably. They aim for different degrees of joining and surface shape. Use a schedule intended for the result you want; a tack fuse is not always achieved simply by using a full-fuse schedule with an arbitrarily shorter hold.
How long should Bullseye glass be annealed?
The annealing hold and cooling rate depend chiefly on the effective thickness and form of the finished piece. Consult the applicable Bullseye annealing guidance and account for the thickest section, rather than choosing a hold based only on the thickness of a single sheet.
Can I fire Bullseye glass with another brand?
Only if the materials are confirmed compatible for the intended kilnforming use. Similar appearance or nominal expansion numbers are not enough to establish compatibility. Check the manufacturers’ technical information before combining them.
Why did my Bullseye piece crack after firing?
Possible causes include inadequate annealing, cooling too quickly, thermal shock, uneven thickness, or incompatible glass. Review the entire schedule and construction, not just the peak temperature, and seek technical guidance for thick or complex pieces.
Using a Schedule as a Starting Point
The most dependable approach is to match the schedule to the project, follow the glass and kiln manufacturers’ current instructions, and keep a record of what actually happened. Treat published schedules as informed starting points for stated conditions, not guarantees for every kiln or every load. With compatible materials, careful preparation, appropriate annealing, and small controlled tests, it becomes easier to repeat a result and understand which adjustments are justified.
Related
- Excel Power Query: Share a File and Control Access
- Equipment Checklist Template Excel: Build a Reliable Tracker
- Event Checklist Template Excel: Build and Use One
Try it: the Date Difference Calculator: days, months, years and weekdays between two dates, with the DATEDIF formulas.
More in How-to basics
- Import a CSV File into Excel: Steps, Settings, and FixesTo import a CSV file into Excel for Microsoft 365 on Windows, open a workbook, select Data >…
- Delete a Page in Word: Can You Remove One?Yes. In Word for Microsoft 365, you can select the contents of a page and delete them, but…
- How to Insert a Checkbox in Word for Forms and ListsTo insert a clickable checkbox in a Word document, turn on the Developer tab, then choose Developer >…
- Can AI Replace Excel Jobs? The Work It Can DoAI can replace some repetitive tasks done in Excel, and in certain workplaces it may reduce the need…
- Excel PivotTable Testing: Checks, Steps, and Common FixesTo test an Excel PivotTable, compare its results with a small source dataset whose totals you can verify…
- Insert a Date in Excel With a Calendar Date PickerTo insert a date by choosing it on a calendar in Excel for Microsoft 365 on Windows, add…
Sources: Function behaviour and menu paths: Microsoft Support documentation for Excel. Method & sources
Spotted an error in this guide? Let us know.