Bullseye Glass Firing Schedules: Temperatures and Tips

How-to basics · Updated November 22, 2026

Bullseye glass firing schedules depend on the project, glass thickness, kiln, and desired finish; there is no single schedule that works for every piece. As a starting point, slumping often uses lower peak temperatures than fusing, while a full fuse commonly reaches roughly 1450–1500°F (788–816°C); use Bullseye’s current schedule guidance and anneal for the thickest part of the piece.

What a firing schedule controls

A kiln schedule is a sequence of heating and cooling steps. Each step usually specifies a ramp rate, a target temperature, and a hold time. The kiln controller follows those instructions, but the glass responds to the temperature it actually experiences, which can differ across the shelf or inside a loaded kiln. The schedule therefore controls more than whether the surface looks melted: it also affects how evenly the glass heats, how air escapes, how much the edges round, and whether the finished work retains stress.

Bullseye glass is commonly described as tested-compatible within its own system, but compatibility does not make every combination of thicknesses, shapes, and firing histories behave identically. A piece that looks fused can still contain damaging stress if it was cooled too quickly. Conversely, holding at a high temperature too long can cause excessive flow, distortion, or devitrification. A sound schedule balances the desired shape with careful heating and cooling.

Know the firing stages

Most kilnforming schedules can be understood as a few functional stages. The controller’s display may use different labels, but the purposes are broadly similar:

  • Initial heat-up: A controlled ramp helps the work warm more evenly. Slower heating is often prudent for thick, large, uneven, or moisture-sensitive loads.
  • Bubble-release stage: Some projects benefit from a slower ramp and a hold below the main fusing temperature so trapped air has time to escape. It is not necessary for every simple, thin construction.
  • Process temperature and hold: The peak and soak produce the intended result, such as a slump, tack fuse, or full fuse. Both time and temperature affect the degree of movement.
  • Cooling to annealing temperature: The kiln must bring the piece to the appropriate annealing range without creating a damaging temperature difference through the glass.
  • Annealing soak and controlled cooling: A hold allows temperature differences to even out; a measured descent through the critical cooling range reduces residual stress.

Do not treat a fast programmed drop from the peak as harmless simply because the kiln is cooling. The period around annealing and strain temperatures is especially important to the durability of the finished glass.

Choose the schedule by the finish you want

Decide what the glass should look and feel like before selecting a schedule. Approximate peak ranges are useful for orientation, not guarantees: actual results depend on the kiln, shelf arrangement, glass thickness, and soak. A lower peak or shorter hold usually limits movement; more heat work generally softens edges and increases flow.

  • Slumping: The glass bends into or over a mold while retaining much of its original surface and layer definition. Slumping commonly takes place around 1200–1250°F (649–677°C), but the mold, shape, and desired depth matter.
  • Tack fusing: Pieces attach while retaining distinct, raised shapes. A broad working range is roughly 1300–1400°F (704–760°C); a small change in heat work can noticeably alter the result.
  • Contour fusing: Edges soften and the surface becomes more integrated, while some original contours remain. It falls between a tack fuse and a full fuse, rather than being a single universal temperature.
  • Full fusing: Layers soften enough to form a more unified, flatter surface. Roughly 1450–1500°F is a common reference range, but a long hold at the low end can produce a different result from a brief hold at the high end.

These are practical starting ranges, not promises of a particular finish. A kiln that fires hot or has a hot spot may produce more movement than another kiln at the same controller setting. Use a test tile when the exact edge profile or degree of fusion matters.

Adjust for thickness, size, and construction

Thickness is central to both heating and annealing. A single layer of glass, a two-layer blank, and a piece with a locally thick stack do not behave as equivalent loads. For annealing, base the schedule on the thickest effective section, not merely the overall length or the average thickness. A small inclusion stack can create a thicker region that needs more careful annealing than the surrounding sheet.

Large pieces can develop greater temperature differences between their centers and edges than small pieces. Uneven construction, narrow necks, sharp corners, and abrupt changes in thickness also deserve caution because they can concentrate stress. A thick blank may need a slower initial ramp, a longer annealing soak, and slower cooling through the critical range than a thin project. Bullseye’s annealing guidance provides thickness-based recommendations; consult the current chart rather than guessing a soak time.

Other factors include how tightly the kiln is loaded, the amount of shelf space around the work, the mold material, and whether the glass is supported evenly. A schedule copied from a small test piece may not transfer directly to a large platter. Keep notes about the glass, dimensions, kiln, shelf position, schedule, and result so you can make informed adjustments.

Use Bullseye charts as the starting authority

For a specific Bullseye product or a schedule intended to follow manufacturer guidance, check Bullseye’s current kilnforming resources and product information. Charts can be updated, and different chart formats may address different thicknesses or operations. Confirm whether temperatures are shown in Fahrenheit or Celsius and whether the listed ramp rate is per hour. Also check the chart’s assumptions: a schedule intended for a particular thickness or simple stack is not automatically suitable for a thick, irregular, or unusually large piece.

Controller settings are not perfectly interchangeable between kilns. Elements, insulation, thermocouple placement and condition, kiln shape, and loading can all affect how closely the glass follows the indicated temperature. If a schedule works reliably in one kiln, treat it as a baseline for that kiln, not a manufacturer-approved universal recipe. For a new kiln, confirm the controller and thermocouple are functioning properly and run small, low-risk tests before committing valuable work.

Test and refine without changing everything

A small test is the safest way to learn how a particular kiln responds. Make a tile using the same glass arrangement and approximate thickness as the intended project. If possible, include a few shapes or edge conditions that reveal how much the glass rounds. Record the schedule and inspect the result after the kiln is fully cool. Change one variable at a time—such as peak temperature, hold duration, or ramp rate—so you can tell which adjustment affected the outcome.

When the glass is underfired, the layers may remain more distinct or the edges may be less rounded than intended. A small increase in peak temperature or hold may add heat work, but either change can increase flow. If the result is overfired, reduce heat work and check whether the kiln’s actual firing behavior differs from its display. Do not compensate for every defect by simply changing the peak: bubbles, kiln wash, glass cleanliness, and mold design can create problems that a hotter or cooler schedule will not fix.

Common problems and practical checks

  • Cracks after firing: Consider inadequate annealing, a thick spot, uneven cooling, or a sharp change in shape. Review the thickness-based annealing guidance and avoid opening the kiln while the work is still hot.
  • Trapped bubbles: Check how the layers are arranged, whether air has an escape path, and whether a suitable bubble-release stage is needed. A longer high-temperature hold can enlarge bubbles rather than remove them.
  • Excessive spreading or rounded edges: The glass may have received too much heat work for the intended finish. Lower the peak or shorten the hold in a controlled test.
  • Uneven slump or inconsistent finish: Check mold level, glass placement, kiln hot spots, and loading. A schedule alone cannot correct an uneven mold or a temperature gradient.
  • Cloudy or rough surface: Review glass cleanliness, kiln wash or separator condition, and firing conditions. Do not assume that every surface defect is caused by an incorrect peak temperature.

Safety while firing

Wear eye protection and gloves when handling sharp glass, and use appropriate precautions when cutting or grinding it. Operate the kiln according to its manufacturer’s instructions, keep combustibles away, and provide the ventilation recommended for the kiln and materials in use. Do not reach into a hot kiln or open it to speed cooling; thermal shock can damage the work, and hot kiln components can cause serious burns. Let the kiln cool to a safe temperature before unloading, and follow the safety instructions for molds, kiln furniture, and any coatings used.

Frequently Asked Questions

What temperature should I full fuse Bullseye glass?
A rough reference range is 1450–1500°F, but the result depends on the kiln, thickness, and hold time. Use Bullseye’s current schedule guidance and test a sample if you need a particular profile.

Can I use the same schedule for tack fusing and full fusing?
Usually not if you want distinct finishes. Tack fusing preserves more raised detail, while full fusing produces greater integration and flow. They typically use different amounts of heat work.

How long should Bullseye glass anneal?
There is no one soak time for every project. Use the manufacturer’s thickness-based annealing chart, taking the thickest part of the piece into account, then follow its controlled cooling guidance.

Can Bullseye glass be fired with other glass?
Use glass that is tested compatible with the Bullseye glass in the project. A similar stated COE alone is not enough to establish compatibility; check the manufacturers’ information before combining systems.

Why did my glass crack even though I followed a schedule?
The schedule may not have suited the piece’s thickness, size, or kiln, or the glass may have experienced uneven heating or cooling. Also inspect for abrupt thickness changes and other stress points, and review the kiln’s actual performance.

Related

Try it: the Date Difference Calculator: days, months, years and weekdays between two dates, with the DATEDIF formulas.

More in How-to basics

Sources: Function behaviour and menu paths: Microsoft Support documentation for Excel. Method & sources

Spotted an error in this guide? Let us know.